Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 250 MPa
36300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 21MB621 OPP Film
Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an..
Film Tensile Strength at Break, TD 250 MPa
36300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 21MB866 OPP Film
Product Description: Bicor 21MB866 is a high gas barrier, transparent biaxially oriented polypropylene film coated on side acrylic, one side PVOH. It provides excellent gas and aroma protection and ..
Film Tensile Strength at Break, TD 250 MPa
36300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 21MBT621 OPP Film
Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both side. The static resistant feature of this film prevents the attraction of dust, and..
Film Tensile Strength at Break, TD 250 MPa
36300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 26MB600 OPP Film
Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia..
Film Tensile Strength at Break, TD 250 MPa
36300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 32MB600 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As..
Film Tensile Strength at Break, TD 250 MPa
36300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Label-Lyte™ 35LH247 OPP Film
Product Description: A super white opaque, caviated BOPP film for Pressure Sensitive (PSA) labeling applications where superior optics are desired. LH247 also shows excellent performance on reel-fed..
Film Tensile Strength at Break, TD 250 MPa
36300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 35HM247 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial..