Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 250 MPa | 36300 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 21MB621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an.. |
|||
Film Tensile Strength at Break, TD | 250 MPa | 36300 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 21MB866 OPP Film Product Description: Bicor 21MB866 is a high gas barrier, transparent biaxially oriented polypropylene film coated on side acrylic, one side PVOH. It provides excellent gas and aroma protection and .. |
|||
Film Tensile Strength at Break, TD | 250 MPa | 36300 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 21MBT621 OPP Film Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both side. The static resistant feature of this film prevents the attraction of dust, and.. |
|||
Film Tensile Strength at Break, TD | 250 MPa | 36300 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 26MB600 OPP Film Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia.. |
|||
Film Tensile Strength at Break, TD | 250 MPa | 36300 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 32MB600 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As.. |
|||
Film Tensile Strength at Break, TD | 250 MPa | 36300 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 35LH247 OPP Film Product Description: A super white opaque, caviated BOPP film for Pressure Sensitive (PSA) labeling applications where superior optics are desired. LH247 also shows excellent performance on reel-fed.. |
|||
Film Tensile Strength at Break, TD | 250 MPa | 36300 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Oppalyte™ 35HM247 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial.. |