Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, TD = 2500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
ASTM D882
M. Holland Company EV200 EVA  (discontinued **)
Features: Good Heat Seal, Opticals, High StrengthUses: PackagingApprovals: FDA 21 CFR 177.1350 and FDA 21 CFR 176.170,Table 2, Cond. C, D, E, F, GProcessing Method: Film, BlownInformation provided b..
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
ASTM D882
LyondellBasell Petrothene® NA143063 Low Density Polyethylene
ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration..
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
Blown; ASTM D822
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
ASTM D882
LyondellBasell Petrothene® NA951000 Low Density Polyethylene
ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab..
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
Blown; ASTM D822
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
ASTM D882
Westlake EP413 Low Density Polyethylene
WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,..
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
ASTM D882
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin
Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through..
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
ASTM D882
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin
Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi..
Film Tensile Strength at Break, TD 17.2 MPa
2500 psi
ASTM D882
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate
Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It can produce f..
Copyright © lookpolymers.com All Rights Reserved