Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | ASTM D882 |
M. Holland Company EV200 EVA
(discontinued **) Features: Good Heat Seal, Opticals, High StrengthUses: PackagingApprovals: FDA 21 CFR 177.1350 and FDA 21 CFR 176.170,Table 2, Cond. C, D, E, F, GProcessing Method: Film, BlownInformation provided b.. |
|||
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | ASTM D882 |
LyondellBasell Petrothene® NA143063 Low Density Polyethylene ApplicationsPETROTHENE NA 143 is a series of homopolymer resins for blown film. Applications include stiff liners. Regulatory StatusNA 143 meets the requirements of the Food and Drug Administration.. |
|||
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | Blown; ASTM D822 |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | ASTM D882 |
LyondellBasell Petrothene® NA951000 Low Density Polyethylene ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab.. |
|||
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | Blown; ASTM D822 |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | ASTM D882 |
Westlake EP413 Low Density Polyethylene WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,.. |
|||
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | ASTM D882 |
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | ASTM D882 |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Film Tensile Strength at Break, TD | 17.2 MPa | 2500 psi | ASTM D882 |
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It can produce f.. |