Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
LyondellBasell Petrothene® NA420127 Low Density Polyethylene
(discontinued **) ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 324 is a series of homopolymer resins specifically designed for overwrap packaging. NA 324 provides excellent optical properties and good stiffness for improved machineabi.. |
|||
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
LyondellBasell Petrothene® NA420000 Low Density Polyethylene ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
LyondellBasell Petrothene® NA960000 Low Density Polyethylene ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif.. |
|||
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
LyondellBasell Petrothene® NA960070 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
LyondellBasell Petrothene® NA960083 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
LyondellBasell Petrothene® NA963083 Low Density Polyethylene ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen.. |
|||
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with e.. |
|||
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
Dow INTEGRAL™ 917 Monolayer Bonding Film INTEGRAL 917 Adhesive Film is a single layer adhesive film for use where a higher flow rate and lower melt point are required. It is useful for bonding heat sensitive materials, or for porous subst.. |