Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 21.0 g/micron | 533 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin Film Properties. Features: Excellent stiffness, excellent puncture, high strength and toughness.Applications: Industrial packaging, overwrap, narrow die gap extrusion.Data provided by the manufactu.. |
|||
Elmendorf Tear Strength, TD | 21.0 g/micron | 533 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANCEED® mL2764 Linear low density polyethylene resin
(discontinued **) Titanceed® mL2764 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL2764 have outstanding tensile properties, impact streng.. |
|||
Elmendorf Tear Strength, TD | 21.0 g/micron | 533 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 10A Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, easy processability, excellent clarity.Applications: Blending resin for improved toughness.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 21.0 g/micron | 533 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 10B Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, excellent dart impact, excellent clarity.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 21.0 g/micron | 533 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |