Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
ASTM D1922
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin  (discontinued **)
Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength ..
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
ASTM D1922A
LyondellBasell Montell 12C01G2 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f..
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
ASTM D1922A
LyondellBasell Montell 12C01G3 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: ..
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
ASTM D1922A
LyondellBasell Montell 12C01G4 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati..
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
ASTM D1922A
LyondellBasell Montell 12C01G5 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl..
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
ASTM D1922A
LyondellBasell Adflexâ„¢ Q 401 F TPO Resin
Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requ..
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
Method A; ASTM D1922
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin
Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1..
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
Westlake LF2050 Hexene Linear Low Density Polyethylene
Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..