Material Notes:
Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requiring resistance to steam sterilization, autoclavable biohazard waste bags, auto masking, heavy duty bags, modified atmosphere packagingMeets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600.Description: Adflex Q 401 F thermoplastic olefin resin with slip and antilock, is designed for aired quenched blown film applications. It is based on proprietary Montell process technology. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792B
Thickness 50.8 microns
2.00 mil
Melt Flow 0.65 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.65 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
Film Elongation at Break, MD 670 %
670 %
ASTM D882
Film Elongation at Break, TD 870 %
870 %
ASTM D882
Secant Modulus, MD 0.331 GPa
48.0 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.304 GPa
44.1 ksi
2% Secant; ASTM D882
Elmendorf Tear Strength MD 440 g
440 g
ASTM D1922A
Elmendorf Tear Strength TD 920 g
920 g
ASTM D1922A
Elmendorf Tear Strength, MD 8.66 g/micron
220 g/mil
ASTM D1922A
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
ASTM D1922A
Dart Drop 10.8 g/micron
275 g/mil
ASTM D1709
Dart Drop Test 550 g
1.21 lb
ASTM D1709A
Film Tensile Strength at Break, MD 68.3 MPa
9910 psi
ASTM D882
Film Tensile Strength at Break, TD 48.3 MPa
7010 psi
ASTM D882
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 152 °C
306 °F
Heat Resistance per Montell