Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Adflexâ„¢ Q 402 F Polyolefin

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer LyondellBasell
Trade Name Adflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Adflexâ„¢ Q 402 F Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Adflex™ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, except for certain fatty foods. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Film property values shown were determined on 2.0 mil thickness blown film extruded at 460°F, 2.5:1 BUR, with a 80 mil die gap. Uses: Film, heavy duty bags, packagingInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.892 g/cc
0.0322 lb/in³
ASTM D792
Thickness 50.8 microns
2.00 mil
Melt Flow 0.65 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.65 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 17.9 MPa
2600 psi
ASTM D882
Film Tensile Strength at Yield, TD 15.2 MPa
2200 psi
ASTM D882
Film Elongation at Break, MD 670 %
670 %
ASTM D882
Film Elongation at Break, TD 870 %
870 %
ASTM D882
Secant Modulus, MD 0.330 GPa
47.9 ksi
2% Secant, 2 mil; ASTM D882
Secant Modulus, TD 0.303 GPa
43.9 ksi
2% Secant, 2 mil; ASTM D882
Elmendorf Tear Strength, MD 8.66 g/micron
220 g/mil
Method A; ASTM D1922
Elmendorf Tear Strength, TD 18.1 g/micron
460 g/mil
Method A; ASTM D1922
Dart Drop 10.8 g/micron
275 g/mil
Method A; ASTM D1709
Film Tensile Strength at Break, MD 68.3 MPa
9900 psi
ASTM D882
Film Tensile Strength at Break, TD 48.3 MPa
7000 psi
ASTM D882
Descriptive Properties Value Comments
Heat Resistance 305°F
Basell Test Method
Puncture Resistance 160 ft-lb/in3
Basell Test Method