Lotte Chemical Titan TITANZEX® HF7000 High density polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANZEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANZEX® HF7000 High density polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HF7000 is a high density polyethylene resin for tubular film extrusion. HF7000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Applications: Very thin reinforcing film Grocery bags Merchandize bags Disposal waste bags Shopping bagsAdvantages: Excellent process ability Excellent draw down capability High film strength and rigidityInformation provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Thickness 17.0 microns
0.669 mil
extruded at 4:1 BUR
Base Resin Melt Index 0.050 g/10 min
0.050 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 250 %
250 %
ASTM D882
Film Elongation at Break, TD 660 %
660 %
ASTM D882
Elmendorf Tear Strength, MD 0.300 g/micron
7.62 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 3.00 g/micron
76.2 g/mil
ASTM D1922
Dart Drop 11.0 g/micron
279 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 78.5 MPa
11400 psi
ASTM D882
Film Tensile Strength at Break, TD 53.9 MPa
7820 psi
ASTM D882
1% Secant Modulus, MD 1276 MPa
185000 psi
ASTM D882
1% Secant Modulus, TD 1179.0 MPa
171000 psi
ASTM D882
Processing Properties Metric English Comments
Melt Temperature 180 - 240 °C
356 - 464 °F
Blow-up Ratio (BUR) 4.0
4.0