Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 12.7 g/micron | 323 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 3 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b.. |
|||
Elmendorf Tear Strength, MD | 12.7 g/micron | 323 g/mil | ISO 6383/2 |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Elmendorf Tear Strength, MD | 12.7 g/micron | 323 g/mil | ISO 6383/2 |
Borealis FA6224 Low Density Polyethylene FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f.. |