Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 68.9 - 82.7 MPa | 10000 - 12000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OEB (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Extra Barrier is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of .. |
|||
Film Tensile Strength at Yield, TD | 68.9 - 82.7 MPa | 10000 - 12000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OEB (1.0 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Extra Barrier is a 1.00 (25micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relat.. |
|||
Film Tensile Strength at Yield, TD | 37.2 - 82.7 MPa | 5400 - 12000 psi | Average value: 65.6 MPa Grade Count:10 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |