Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin
(discontinued **) Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | ASTM D882 |
Westlake Mxsten CV77512 Polyethylene Plastomer Mxsten CV plastomer CV77512 is a polyethylene plastomer designed for blown film extrusion that contains high slip, high antiblock and high processing aid additives. Films produced with this resin ex.. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | ASTM D882 |
Westlake Mxsten CV77523 Polyethylene Plastomer Mxsten CV plastomer CV77523 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this .. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | ASTM D882 |
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope.. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit.. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, TD | 7.58 MPa | 1100 psi | ASTM D882 |
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior p.. |