Polymer Property : Film Tensile Strength at Yield, TD = 3630 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD >= 25.0 MPa
>= 3630 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD 25.0 MPa
3630 psi
Cast Film; ASTM D638
Chevron Phillips Marlex® HHM TR-166 Polyethylene, Film Grade; HDPE  (discontinued **)
FDA approved.Data provided by the manufacturer
Film Tensile Strength at Yield, TD 25.0 MPa
3630 psi
ASTM D 882
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin
HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che..
Film Tensile Strength at Yield, TD 25.0 MPa

@Temperature 23.0 °C
3630 psi

@Temperature 73.4 °F
ASTM D638
Mapal Plastics Maplon Type H Polypropylene Sheet
Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.Applications : Stationery, Printing..
Film Tensile Strength at Yield, TD 25.0 MPa
3630 psi
ASTM D882
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film
Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor..
Film Tensile Strength at Yield, TD 25.0 MPa
3630 psi
ISO 527-3
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
This product is a Total Ecosolutions grade.Lumicene® mPE M 4707 EP is a second generation metallocene based High Density Polyethylene with hexene as comonomer.Lumicene® mPE M 4707 EP can be proces..
Film Tensile Strength at Yield, TD 25.0 - 30.0 MPa
3630 - 4350 psi
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents..
Film Tensile Strength at Yield, TD 25.0 MPa
3630 psi
ISO 527-3
EMS-Grivory Grivory® BM 17 PA*
Product description: Grilon BM 17 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 17 natural has the following features: High flexibility and toughnessVery good ori..