Film Tensile Strength at Yield, TD 8.00 - 18.0 MPa
1160 - 2610 psi
Average value: 10.9 MPa Grade Count:48
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum..
Film Tensile Strength at Yield, TD 15.0 - 18.0 MPa
2180 - 2610 psi
Average value: 16.9 MPa Grade Count:16
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and..