Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
at 2% offset; ASTM D882
ExxonMobil Exceed™ 1023CA Tough Premium Film Resin  (discontinued **)
Exceed 1023CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023CA resin have outstanding tensile, impact strength and puncture. These superi..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
LyondellBasell Petrothene® M2520FN Low Density Polyethylene
ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LD 123.LN General Purpose Clarity Film Resin
Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America ..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin
Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America ..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin
Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin
Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part..
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st..