ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesApplications: Bread BagsCo-Extrusion FilmsCollation ShrinkDiaper BacksheetFoamsHigh Performance Collation ShrinkHygiene PackagingLabel FilmLamination FilmOverwrap FilmPaper Overwrap Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ExxonMobil method
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.7 MPa
1700 psi
ASTM D882
Film Elongation at Break, MD 270 %
270 %
ASTM D882
Film Elongation at Break, TD 660 %
660 %
ASTM D882
Puncture Energy 2.03 J
1.50 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 480 g
480 g
ASTM D1922
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
Dart Drop Test 100 g
0.221 lb
ASTM D1709A
Film Tensile Strength at Break, MD 28.3 MPa
4100 psi
ASTM D882
Film Tensile Strength at Break, TD 24.1 MPa
3500 psi
ASTM D882
1% Secant Modulus, MD 221 MPa
32000 psi
ASTM D882
1% Secant Modulus, TD 269 MPa
39000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 234 °C
<= 453 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 5.3 %
5.3 %
ASTM D1003
Gloss 72 %
72 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 13 lbf
ExxonMobil Method