Polymer Property : Shear Modulus = 79.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 79.0 GPa
11500 ksi
Special Metals INCONEL® C276 Nickel Superalloy Bar
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special ..
Shear Modulus 79.0 GPa
11500 ksi
Special Metals INCONEL® C276 Nickel Superalloy Plate
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia..
Shear Modulus 79.0 GPa
11500 ksi
Special Metals INCONEL® C276 Nickel Superalloy Sheet
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed sheet. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia..
Shear Modulus 79.0 GPa
11500 ksi
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed)
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci..
Shear Modulus 79.0 GPa
11500 ksi
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Shear Modulus 79.0 GPa
11500 ksi
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Shear Modulus 79.0 GPa
11500 ksi
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Shear Modulus 79.0 GPa
11500 ksi
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
Shear Modulus 79.0 GPa
11500 ksi
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
Shear Modulus 79.0 GPa
11500 ksi
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range), Heat Treated
Heat Treatment 5 hours at 527°C. 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below ar..
Shear Modulus 79.0 GPa
11500 ksi
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..