Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 79.0 GPa | 11500 ksi | |
Special Metals INCONEL® C276 Nickel Superalloy Bar Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special .. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Special Metals INCONEL® C276 Nickel Superalloy Plate Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Special Metals INCONEL® C276 Nickel Superalloy Sheet Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed sheet. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed) Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range), Heat Treated Heat Treatment 5 hours at 527°C. 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below ar.. |
|||
Shear Modulus | 79.0 GPa | 11500 ksi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |