Mechanical Properties Metric English Comments
Shear Modulus 5.40 GPa
783 ksi
Calculated
Premix Premi-Glas® 1100-10 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-10 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Shear Modulus 5.40 GPa
783 ksi
Calculated
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Shear Modulus 5.40 GPa
783 ksi
Calculated
Premix Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Shear Modulus 5.40 GPa
783 ksi
Calculated
Premix Premi-Glas® 1100-25 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Shear Modulus 5.40 GPa
783 ksi
Calculated
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
Shear Modulus 5.40 GPa
783 ksi
Calculated
Premix Premi-Glas® 1100V-15 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-15 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
Shear Modulus 5.40 GPa
783 ksi
Calculated
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
Shear Modulus 5.40 GPa
783 ksi
Calculated
Premix Premi-Glas® 1286 Glass Reinforced SMC
Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding..
Shear Modulus 5.40 GPa
783 ksi
in plane
Menzolit Menzolit® BMC 0390 Unsaturated Polyester UP
BMC 0390 is a low profile DMC/BMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surface qua..
Shear Modulus 5.40 GPa
783 ksi
in plane
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP
BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac..
Shear Modulus 5.40 GPa
783 ksi
in plane
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP
BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of ..
Shear Modulus 5.40 GPa
783 ksi
in plane
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP
BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific..
Shear Modulus 5.40 GPa
783 ksi
in plane
Menzolit Menzolit® BMC 3000 Unsaturated Polyester UP
BMC 3000 is a special BMC suitable for the use in microwave and cookware applications.It has high temperature resistance, and meets requirements for food contact applications. It has a high gloss fi..
Shear Modulus 5.40 GPa
783 ksi
in plane
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP
BMC 3100 is a special BMC suitable for the use in head lamp reflectors. Because of its high temperature resistance and dimensional stability as well as low coefficient of thermal expansion, complex ..