Mechanical Properties Metric English Comments
Shear Modulus 0.0138 - 0.3656 GPa

@Temperature -50.0 - 0.000 °C
2.00 - 53.03 ksi

@Temperature -58.0 - 32.0 °F
Average value: 0.159 GPa Grade Count:1
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..