Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Modulus = 0.0138 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.0138 - 0.3656 GPa

@Temperature -50.0 - 0.000 °C
2.00 - 53.03 ksi

@Temperature -58.0 - 32.0 °F
Average value: 0.159 GPa Grade Count:1
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Shear Modulus 0.0138 GPa
2.00 ksi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-10/OX - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Modulus 0.0138 GPa
2.00 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 1/2 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Modulus 0.0138 GPa
2.00 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 1/4 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Copyright © lookpolymers.com All Rights Reserved