Polymer Property : Shear Modulus = 4.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 4.10 GPa
595 ksi
calculated
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is..
Shear Modulus 4.10 GPa
595 ksi
EN6031
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/35%/UD134/AS7-12K
Fiber: AS7, Weave: UD, 134 g/m2Information provided by HexCel
Shear Modulus 4.10 GPa
595 ksi
EN6031
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/280H5/AS4-3K
Fiber: AS, Weave: 5HS, 280 g/m2Information provided by HexCel