Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/35%/UD134/AS7-12K

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/35%/UD134/AS7-12K.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiber: AS7, Weave: UD, 134 g/m2Information provided by HexCel
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Cured Resin
1.51 g/cc
0.0546 lb/in³
Nominal Laminate
1.79 g/cc
0.0647 lb/in³
Fibre
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2330 MPa
338000 psi
EN2597B
Tensile Modulus 141 GPa
20500 ksi
EN2597B
Compressive Yield Strength 1308 MPa
189700 psi
EN2850B
Compressive Modulus 129 GPa
18700 ksi
EN2850B
Shear Modulus 4.10 GPa
595 ksi
EN6031
Shear Strength 94.4 MPa
13700 psi
ILSS; EN2563
115 MPa
16700 psi
In-Plane; EN6031
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 197 °C
387 °F
EN6032
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0137
Fiber Volume (%) 54.8
Nominal