Mechanical Properties Metric English Comments
Shear Modulus 0.900 - 0.980 GPa
131 - 142 ksi
Average value: 0.940 GPa Grade Count:5
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Shear Modulus 0.900 GPa
131 ksi
DIN 53457
Global PP-1111-R Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-electrical/electronic Information provided by Global Polymers Corporation.
Shear Modulus 0.900 GPa
131 ksi
ISO 6721-2
Styrolution Luran® S 757 G Q43 White 36609 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
Shear Modulus 0.900 GPa
131 ksi
ISO 6721-2
Styrolution Luran® S 757 G UV White 37019 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
Shear Modulus 0.900 GPa
131 ksi
ISO 6721-2
Styrolution Luran® S 757 R Colored ASA
Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Shear Modulus 0.900 GPa
131 ksi
ISO 6721-2
Styrolution Polystyrol 454 C GR 2 PS
Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts..
Shear Modulus 0.900 GPa
131 ksi
calculated
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)  (discontinued **)
Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions..
Shear Modulus 0.900 GPa
131 ksi
ISO 6721-2
Styrolution Luran® S KR 2861/1 C Colored ASA+PC
Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh..