Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.900 - 0.980 GPa | 131 - 142 ksi | Average value: 0.940 GPa Grade Count:5 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Shear Modulus | 0.900 GPa | 131 ksi | DIN 53457 |
Global PP-1111-R Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-electrical/electronic Information provided by Global Polymers Corporation. |
|||
Shear Modulus | 0.900 GPa | 131 ksi | ISO 6721-2 |
Styrolution Luran® S 757 G Q43 White 36609 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Shear Modulus | 0.900 GPa | 131 ksi | ISO 6721-2 |
Styrolution Luran® S 757 G UV White 37019 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Shear Modulus | 0.900 GPa | 131 ksi | ISO 6721-2 |
Styrolution Luran® S 757 R Colored ASA Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Shear Modulus | 0.900 GPa | 131 ksi | ISO 6721-2 |
Styrolution Polystyrol 454 C GR 2 PS Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts.. |
|||
Shear Modulus | 0.900 GPa | 131 ksi | calculated |
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions.. |
|||
Shear Modulus | 0.900 GPa | 131 ksi | ISO 6721-2 |
Styrolution Luran® S KR 2861/1 C Colored ASA+PC Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh.. |