Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 72.4 GPa | 10500 ksi | |
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |
|||
Shear Modulus | 72.3 GPa | 10500 ksi | |
Crucible Steel 416R Chromium Stainless Steel Crucible 416R is a pre-hardened chromium stainless steel which is suitable for use in precision match-grade rifle barrels. It can be supplied in various hardness ranges according to the specific req.. |
|||
Shear Modulus | 72.1 GPa | 10500 ksi | Calculated |
Carpenter 20-Mo6® Stainless Steel, Plate Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Shear Modulus | 72.1 GPa | 10500 ksi | Calculated |
Carpenter 20-Mo6® Stainless Steel, Strip Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Shear Modulus | 72.1 GPa @Temperature 23.0 °C |
10500 ksi @Temperature 73.4 °F |
|
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Shear Modulus | 72.3 GPa | 10500 ksi | Calculated |
Ceradyne Ceralloy® 147-1B Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |