Mechanical Properties Metric English Comments
Tensile Modulus 9.28 GPa
1350 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC
LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi..
Tensile Modulus 9.28 GPa
1350 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXJ PC
LNP* Lubricomp* DFL36XXJ is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare..
Tensile Modulus 9.28 GPa
1350 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific)
LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Tensile Modulus 9.28 GPa
1350 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific)
LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber.
Tensile Modulus 9.28 GPa
1350 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11
LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber.