Mechanical Properties Metric English Comments
Tensile Modulus 9.16 GPa
1330 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DE0021E PC
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive.
Tensile Modulus 9.16 GPa
1330 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific)
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding.
Tensile Modulus 9.16 GPa
1330 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton PV007SV_WH8D537 PA 6
Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region.