Mechanical Properties Metric English Comments
Tensile Modulus 5.97 GPa
866 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific)
LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.This data was suppli..
Tensile Modulus 5.97 GPa
866 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66
LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber.