Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.12 GPa | 743 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
Tensile Modulus | 5.12 GPa | 743 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Tensile Modulus | 5.12 GPa | 743 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF003H PA 66 LNP* THERMOCOMP* RF003H is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 5.12 GPa | 743 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF003XXH PA 66 LNP* THERMOCOMP* RF003XXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 5.12 GPa | 743 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific) This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 5.12 GPa | 743 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02841 PBT+PC LNP* Thermocmop* 9X02841 is a PBT/Polycarbonate blend containing proprietary fillers. |
|||
Tensile Modulus | 5.12 GPa | 743 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 5.12 GPa | 743 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 (Asia Pacific) LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |