Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 6670 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 46.0 GPa
6670 ksi
ISO 527-1
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound
Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)...
Copyright © lookpolymers.com All Rights Reserved