Category Polymer , Thermoset , Epoxy , Epoxy Molding Compound , Filled/Reinforced Thermoset
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name Neopreg Kinel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C). Superior creep resistance and dimensional stability.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Bulk Density 0.350 g/cc
0.0126 lb/in³
ISO 60
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Water Absorption 0.060 %
0.060 %
ISO 62
Linear Mold Shrinkage 0.00020 cm/cm
0.00020 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 148 MPa
21500 psi
ISO 527-1
Elongation at Break 0.30 %
0.30 %
ISO 527-1
Tensile Modulus 46.0 GPa
6670 ksi
ISO 527-1
Flexural Strength 363 MPa
52600 psi
ISO 178
Flexural Modulus 32.0 GPa
4640 ksi
ISO 178
Compressive Strength 230 MPa
33400 psi
ISO 604
Charpy Impact, Notched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 3.30 µm/m-°C
1.83 µin/in-°F
TMA
CTE, linear, Transverse to Flow 40.0 µm/m-°C
22.2 µin/in-°F
TMA
Glass Transition Temp, Tg 195 °C
383 °F
Shrinkage -0.0100 %
-0.0100 %
Post Shrinkage; ISO 2577
Descriptive Properties Value Comments
Color Black
Molding Method Compression
Injection
Transfer
Users viewing this material also viewed the following: