Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 46.0 GPa | 6670 ksi | ISO 527-1 |
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)... |