Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 415 GPa | 60200 ksi | Young's; DINV ENV 843-2 |
CeramTec CD 101 Silicon Carbide, SiC-ZrB2 CD101 is a zirconia reinforced silicon carbide designed for maximum hardness. |
|||
Tensile Modulus | 415 GPa | 60200 ksi | Young's; DINV ENV 843-2 |
CeramTec CD 110 Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati.. |