Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.59 GPa
956 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific)
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 6.59 GPa
956 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.