Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.300 - 0.400 GPa | 43.5 - 58.0 ksi | ISO 527-3 |
Borealis Borseal™ RE239CF Polypropylene Copolymer Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high.. |