Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 0.400 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.300 - 0.400 GPa
43.5 - 58.0 ksi
ISO 527-3
Borealis Borseal™ RE239CF Polypropylene Copolymer
Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high..
Copyright © lookpolymers.com All Rights Reserved