Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.300 GPa | 43.5 ksi | ASTM D638 |
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3020 D LDPE Blow molding, injection molding.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3020 F LDPE Blown film, injection moldings, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3020 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3020 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3024 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3025 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3026 F LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3032 D LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | |
LyondellBasell Lupolen® 3040 D LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC (Asia Pacific) LNP* LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon TD000 LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON TD000 PU LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 0.300 - 0.400 GPa | 43.5 - 58.0 ksi | ISO 527-3 |
Borealis Borseal™ RE239CF Polypropylene Copolymer Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | MD/TD; ISO 527-3 |
Borealis Borseal™ RE939CF Polypropylene Copolymer Borseal™ RE939CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: Borseal™ RE939CF is designed for: Food packaging,.. |
|||
Tensile Modulus | 0.300 GPa @Temperature 100 °C |
43.5 ksi @Temperature 212 °F |
DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | ISO 527-1/-2 |
DSM Arnitel® PB582-H 58 Shore D, Blow Molding Grade, Heat Stabilized Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | ISO 527-1/-2 |
DSM Arnitel® PB582-H Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | ISO 527-1/-2 |
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | ISO 527-1/-2 |
DSM Arnitel® PL581 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | ISO 527-1/-2 |
DSM Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | 1 mm/min |
Arkema Group Orgalloy® LT 4060IH Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (200 MPa), good .. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | ISO 527-1/-2 |
DSM Arnitel® PM581 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.300 GPa | 43.5 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 334 H PA6 Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a.. |