Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.865 GPa | 560.5 ksi | ASTM D638 |
Ensinger Tecapeek® XP-91BST Compression Molded PEEK ST Compound, 30% Fiberglass, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |