Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® XP-91BST Compression Molded PEEK ST Compound, 30% Fiberglass, Black Pigmented

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-91BST Compression Molded PEEK ST Compound, 30% Fiberglass, Black Pigmented.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 106
106
ASTM D785
Tensile Strength 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
Flexural Strain; ASTM D790
2.1 %
2.1 %
ASTM D638
Tensile Modulus 3.865 GPa
560.5 ksi
ASTM D638
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Flexural Modulus 7.93 GPa
1150 ksi
ASTM D790
Compressive Strength 129 MPa
18700 psi
ASTM D695
Compressive Modulus 3.56 GPa
516 ksi
ASTM D695
Izod Impact, Notched 0.112 J/cm
0.210 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: