Polymer Property : Tensile Modulus = 3.865 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.865 GPa
560.5 ksi
ASTM D638
Ensinger Tecapeek® XP-91BST Compression Molded PEEK ST Compound, 30% Fiberglass, Black Pigmented
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..