Polymer Property : Tensile Modulus = 455 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.14 GPa
455 ksi
DIN 53457
Isoflon PMMA Polymethyl-methacrylate
Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon.
Tensile Modulus 3.14 GPa
455 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66
LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.14 GPa
455 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Tensile Modulus 3.14 GPa
455 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL FP6130 PPE+PS
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Tensile Modulus 3.14 GPa
455 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..