Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.649 GPa @Temperature 110 °C |
384.2 ksi @Temperature 230 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |