Tensile Modulus 2.649 GPa

@Temperature 110 °C
384.2 ksi

@Temperature 230 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..