Mechanical Properties Metric English Comments
Tensile Modulus 26.0 GPa
3770 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)  (Unverified Data**)
Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f..
Tensile Modulus 26.0 GPa
3770 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber
Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla..
Tensile Modulus 26.0 GPa
3770 ksi
90º, RT, Dry; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel
Tensile Modulus 26.0 GPa

@Temperature 75.0 °C
3770 ksi

@Temperature 167 °F
90º, Wet; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel
Tensile Modulus 26.0 GPa
3770 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40
Information provided by EMS Grivory
Tensile Modulus 26.0 GPa
3770 ksi
ISO 527
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..