Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber

Category Polymer , Thermoplastic , Polyarylamide (PAA)
Manufacturer Solvay Specialty Polymers
Trade Name Ixef®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-fiber reinforced engineering resins.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Ultra High StiffnessUses: Appliance Components; Appliances; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bushings; Camera Applications; Cams; Cell Phones; Electrical/Electronic Applications; Furniture; Gears; Industrial Applications; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other ToolsInjection Molding Notes: Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding.Automotive Specifications BMW GS 93016Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Filler Content 30 %
30 %
Carbon Fiber
Water Absorption 0.22 %

@Time 86400 sec
0.22 %

@Time 24.0 hour
ISO 62
Water Absorption at Saturation 2.0 %
2.0 %
65% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.00030 - 0.0010 cm/cm
0.00030 - 0.0010 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 250 MPa
36300 psi
ISO 527-2
Elongation at Break 1.3 %
1.3 %
ISO 527-2
Tensile Modulus 26.0 GPa
3770 ksi
ISO 527-2
Flexural Strength 360 MPa
52200 psi
ISO 178
Flexural Modulus 23.0 GPa
3340 ksi
ISO 178
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.50 J/cm
8.43 ft-lb/in
ASTM D256
Charpy Impact Unnotched 3.60 J/cm²
17.1 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.360 J/cm²
1.71 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
Unannealed; ISO 75-2/A
Flammability, UL94 HB
HB
Oxygen Index 23 %
23 %
ISO 4589-2
Electrical Properties Metric English Comments
Volume Resistivity 3000 ohm-cm
3000 ohm-cm
ASTM D257
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 260 °C
482 - 500 °F
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Melt Temperature 280 °C
536 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 120 °C

@Time 1800 - 5400 sec
248 °F

@Time 0.500 - 1.50 hour
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Processing Technique Injection Molding
Copyright © lookpolymers.com All Rights Reserved