Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 22.4 GPa | 3250 ksi | longitudinal; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact .. |
|||
Tensile Modulus | 22.4 GPa | 3250 ksi | 1mm/min; ISO 527 |
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry) Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil.. |