Mechanical Properties Metric English Comments
Tensile Modulus 22.4 GPa
3250 ksi
longitudinal; ISO 527-4/5
Bond Laminates TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact ..
Tensile Modulus 22.4 GPa
3250 ksi
1mm/min; ISO 527
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry)
Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil..