Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 22.1 GPa | 3200 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ES-40CF/000 Polyethersulfone - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 22.1 GPa | 3200 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ SFC-5000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 22.06 GPa | 3200 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Tensile Modulus | 22.06 GPa | 3200 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific) LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Tensile Modulus | 22.06 GPa | 3200 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Tensile Modulus | 22.06 GPa | 3200 ksi | |
COI Ceramics Friable Graded Insulation Description: An example of a bonded product comprised of oxide spheres is Friable Graded Insulation or FGI. FGI can be bonded to an oxide ceramic matrix composite such as A/N720 to produce a CMC/FGI.. |